彩涂卷為什么會出現(xiàn)爆漆? Why does color paint roll appear to paint? 夏季炎炎,隨著氣溫不斷降低,很多地區(qū)涉及到多種類型的彩涂卷都出現(xiàn)了爆漆現(xiàn)象。 彩涂卷爆漆和天氣真的有關(guān)系嗎?其實這不是全部原因,接下來讓我們談?wù)劜释烤沓霈F(xiàn)爆漆的其他原因。 Summer heat, as the temperature continues to drop, many areas involved in a variety of types of color rolls have appeared paint phenomenon. Is the paint paint really having something to do with the weather? In fact, this is not the whole reason, then let's talk about the other reasons for the paint explosion. 1. 彩涂卷生產(chǎn)工藝中要求,彩涂卷的溫度需要每兩小時檢查一次,如果工作人員沒有按時跟蹤掌握溫度,特別是在冬季,溫度在2小時內(nèi)變化較大,最終會導(dǎo)致涂色時間較長。 1. According to the production process, the temperature of color coating needs to be checked every two hours. If the staff does not track the temperature on time, especially in winter, the temperature changes greatly within 2 hours, which will eventually lead to a long coloring time. 2.在彩涂卷生產(chǎn)過程中,出口檢驗鏡和滾筒上的粉塵會直接營銷顏料的著色效果,剛開始不會特別明顯,在太陽下會完全展現(xiàn)。 2. In the production process of color coating and rolling, the dust on the export inspection mirror and the drum will directly market the coloring effect of the pigment, which will not be particularly obvious at the beginning, but will be fully displayed in the sun. 在施工過程中,彩涂鋼板表面容易被刮花損壞,漆面破損了材料容易被大氣腐蝕生銹,特別在環(huán)境相對惡劣的地方,表面劃傷可通過噴涂修復(fù)劃傷部位,佛山萬慶物資可以給客戶提供相關(guān)修復(fù)技術(shù)支持,歡迎廣大用戶致電13825566148咨詢。 In the construction process of construction, color plate surface is easy to scratch damage, paint damaged material is easy to atmospheric corrosion rust, especially in the environment is relatively bad, surface scratches can by spraying repair scratches, Foshan evergreen materials can provide related repair technical support, welcome users to call 13825566148 consultation. |